Hi Jim- We may still use some with RED dye added, but mostly UV. The red dye was not opaque, but only a tint to help with visual inspection. -Chris TechNet <[log in to unmask]> wrote on 10/19/2006 09:29:26 AM: > Does anyone know of any conformal coating that has a color to it instead > of clear? We are currently spraying some conformal coating manually, > and with it being clear, it is not always guaranteed that the operator > hits all required areas. > > Thanks, > > > > Jim West > Engineering Manager > Nexergy Inc. > www.nexergy.com > tel: (614) 351-6216 > fax: (614) 324-1979 > > > > This email message and all attachments transmitted with it are > intended solely for the use of the addressee(s) and may contain > legally privileged, protected or confidential information. If you > believe that you have received this message in error, please notify > the sender immediately by email reply and please delete this message > from your computer and destroy any copies. > > -------------------------------------------------------- > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 1.8e > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 > for additional information, or contact Keach Sasamori at [log in to unmask] > org or 847-615-7100 ext.2815 > ----------------------------------------------------- > "This e-mail message is intended only for the use of the intended recipient(s). The information contained therein may be confidential or privileged, and its disclosure or reproduction is strictly prohibited. If you are not the intended recipient, please return it immediately to its sender at the above address and destroy it." --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------