OK, case closed. Have to get used to stay at my desk for more than 3 seconds when reading specs. Thanks Ian, Ioan -----Original Message----- From: Ian Hanna [mailto:[log in to unmask]] Sent: Friday, September 22, 2006 9:17 AM To: 'TechNet E-Mail Forum'; Tempea, Ioan Subject: RE: [TN] Thickness of gold in ENIG IPC 4552 Oct 2002 3.2.2 says 1.97 u" min -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Tempea, Ioan Sent: Friday, September 22, 2006 9:03 AM To: [log in to unmask] Subject: [TN] Thickness of gold in ENIG Hi Technos, as per my copy of ICP-4552, dated October 2002, paragraph 3.2.2 recommends 2.955 to 4.925 micro inches of Au. I was challenged on that and would like to know if there is a more recent release of the standard, stating a minimum of 2 micro in. Thanks, Ioan --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------