Hi Ioan! Are you sure that things are really different between the "Leaded" and "Lead-free" parts besides the plating? We were in a situation where we had to build a consigned material assembly which is in the process of becoming "compliant". However, our customer had purchased quite a number of digital video devices and did not want to throw them away because they weren't PB free...the assemblies that we were building weren't going to the EU. But we were using PB free solder paste and had some concerns about whether or not the leaded parts would be able to withstand the lead-free temperatures. So we called the manufacturer of the device inquiring if the part could take the heat, and was told "unofficially" (like if we repeated what he said he would deny it) that the only difference between the lead-free and leaded part was the plating on the leads...nothing had changed internally. I wonder how many PB free parts REALLY have something different about them besides the lead plating? -Steve Gregory- -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Tempea, Ioan Sent: Monday, September 18, 2006 11:26 AM To: [log in to unmask] Subject: [TN] Lower temp soldering pass of lead-free boards Hi Technos, I have a lead-free board, but some nasty leadless comps are only available leaded, so not supporting 240C. I am thinking what about soldering everything that works at lead-free temps and then make another soldering pass at about 210C with these comps only. Will this affect the reliability of the lead-free joints, since the solder will get almost pasty? Did anybody try this? I agree with the ones that will say: "what the heck, they cannot give you compliant parts, don't do it", but it is an important project, the customer knows what this means, but they want to risk. Btw, I have to make sure the original reliability of the lead-free joints, as good as it is, will not be latered, it is a high-rel application. Thanks, Ioan --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------