Inge, Has it been confirmed that the solder spheres are Pb90/Sn10? Or what are they? -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Joe Fjelstad Sent: Tuesday, September 12, 2006 1:26 PM To: [log in to unmask] Subject: Re: [TN] PbCO3 Thanks Inge. (You are working late. A by product of the Nordic affinity for strong coffee perhaps ;-) ? "Curious and curiouser", indeed. Was this a one lot of product effect or is it repeating? If has been limited to one lot, has an attempt been made to recreate the effect in some sort of designed experiment? Obviously based on the scale, the length of these whiskers are not going to be a threat equal to the threat of tin whiskers which can be more than two orders of magnitude greater in length. Nothing like a good process problem to keep the process engineers mental gears engaged. Best regards, Joe --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------