Eric: Whereas IPA may well give you a good clean, it will probably worsen the problems you are seeing with water... And then there might be some minor issues with flammability, and the fact that you will need an explosion proof US cleaner... Other than that, it is a GREAT IDEA... :-) Rudy Sedlak RD Chemical Company Eric CHRISTISON <[log in to unmask]> wrote: We're currently ultrasonically cleaning some plastic parts in DI water and may be incurring some microscopic damage to the surface. We've been directed to use IPA rather than DI water as a cleaning medium to give a gentler clean to reduce damage. Does this sound like a good plan and would there be any other fluids that would be more suitable? Regards, -- Eric Christison Msc Mechanical Engineer Home Personal, Communication Sector Imaging Division STMicroelectronics (R&D) Ltd 33 Pinkhill Edinburgh EH12 7BF United Kingdom Tel: +44 (0)131 336 6165 Fax: + 44 (0)131 336 6001 --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------- Do you Yahoo!? --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- Everyone is raving about the all-new Yahoo! Mail.