Recently I asked an outside lab to perform the dye & pry test on couple failure assemblies. The heatsink was not removed from the PBGA prior to the dye application. According to the result and pictures, the corner pads of the BGA package from both units were covered by the dye completely . An indication that a seperation was formed between the BGA package's pads and its original solder balls at that one corner after the SMT process. Have anyone of you experienced this kind of defects in the past and what could be the root cause of this phenomena? ( Poor plating from the IC manufacturer? SMT reflow profile? PCB warpage? ) I have been in the industry for 10 years and have never seen thing like this. Is it common?? Thanks Ryu --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------