Greetings Technet. I have an interesting problem that has developed since we converted to our lead-free process. We have been using an Electrovert Astrapak for our wave solder operation for many years in our SnPb process. A few months ago, we converted the machine for SAC305 by installing new titanium parts (solderpot, pumps, wave guides, etc) and loaded it up with Alpha metals SAC305. We removed and cleaned up the transport fingers in alcohol while the pot conversion was under way. After putting the machine back together our new lead-free process seemed perfect -- except that now the SAC305 is sticking to the titanium transport fingers- I mean really sticking to them. The smooth wave doesn't seem to affect the fingers as much as the chip wave- but after a run of about 200 PCBs- the fingers are fouled with solder - to the point that we have to stop and brush out the fingers with a rotary wire brush. We never had this problem with leaded solder. We do not have an automatic finger-cleaner installed on the machine (we never had this problem before) and I cannot find one anywhere to retrofit. But the question still comes down to-- what is causing the solder to stick where it did not stick before? We use a no -clean flux (Alpha EF2202 or Indium 1075, makes no difference --the solder still sticks.) The fingers were not changed out (only soaked and cleaned with alcohol) when the rest of the machine was converted to lead-free. Any insight into solving the problem would be greatly appreciated. Neil Maloney, Manufacturing Engineer Contemporary Control Systems, inc 2431 Curtiss St Downers Grove, IL 60515 (630) 963-7070 x132 [log in to unmask] http://www.ccontrols.com <http://www.ccontrols.com/> http://www.ctrlink.com <http://www.ctrlink.com/> --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------