They are the same, 303 SS contains 18% Chromium, 10% Nickel. Franklin -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Charlie Barker Sent: Friday, August 25, 2006 10:59 AM To: [log in to unmask] Subject: [TN] 303 SS vs. 18-10 SS Howdy; Now that all have whetted their thirst for watery subjects, maybe one of you wizards can help me on this: What is the difference in the characteristics or quality, etc. of 18-10 stainless vs. 303 stainless? We need some ¼-16 threaded 303 stainless PDQ. A local supplier can get us some 18-10. Is it better? This is used as a lead screw in an small industrial machine. TIA Charlie B. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------