The processes for REWORK outlined in IPC 7711/7721 are done in order to bring the product back into compliance with IPC-A-610D. If the inspector is certified to 610D then they can inspect the rework. The REPAIRS outlined in this document do not bring the product into print compliance. Some additional material is required that is not on the BOM or assembly drawing, such as wire jumpers, epoxy, etc. The repair brings the product back into form, fit, and functionality, but is still non-compliant material. Therefore review from your Materials Review Board of the damage and inspection of the repair documented on a non-compliant materials report should be performed. Typically you must have MRB authority from your customer for performing repairs, and they may request advance notification and authorization of the usage of any particular repair procedure. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Chafin, Ken G. Sent: Monday, July 10, 2006 8:07 AM To: [log in to unmask] Subject: [TN] IPC-A-610D If one is IPC certified per IPC-A-610 to inspect electronic assemblies, is one thereby recognized as competent to inspect reworked, repaired or modified electronic assemblies (Ref: IPC-7711, IPD-7721). Or is special inspection training required for this per IPC? I don't know if I have asked the question properly but I would be interested in any comments. Thanks --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------