Hi Victor, What's the plating for ? PCB's ? Components? LS -----Original Message----- From: Victor G. Hernandez [mailto:[log in to unmask]] Sent: Wednesday, July 12, 2006 10:14 AM To: [log in to unmask] Subject: Au, PdAu, Ni , base metal plating Fellow TechNetters: Can someone share their experience with the above stated process. I am searching for desired thickness and plating sequence. Is sequence acceptable and the use of Sn? 1. NICKEL THICKESS :50-90''=20 2.Sn THICKNESS:30-50'' OVER NICKEL=20 3.Pd/Ni THCIKNESS:30'' OVER Sn=20 4. GOLD THICKNESS: 5-7'' OVER Pd/Ni=20 Victor, ---------------------------------------------------------------------------- ---Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Leadfree To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL) Search previous postings at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=3D4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ---------------------------------------------------------------------------- --- THIS EMAIL AND ANY ATTACHED FILES ARE CONFIDENTIAL AND MAY BE LEGALLY PRIVILEGED. If you are not the addressee, any disclosure, reproduction, copying, distribution or other dissemination or use of this communication is strictly prohibited. If you have received this transmission in error, please notify the sender immediately and delete this email. It is the policy of ACR Electronics, Inc. that no legally binding statements, representations or commitments (collectively statements) may be made by email. Any such statements must be confirmed either by facsimile transmission or by postal mail before they will have legal effect. The sender of this email is not authorised to commit the company in any way and the addressee is hereby notified of that fact. -------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Leadfree To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL) Search previous postings at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -------------------------------------------------------------------------------