Amol, I am successfully using my old Conceptronic Freedom 2000, vintage 1997. No issue, I have bumped up the regular recipes by 30C and that's it. The only issue I have is when the operators get lead-free BGAs from the stock instead of SnPb, for regular, SnPb rework ;-) And it happens more and more... Not to mention about the joys of having mixed nuts in the same tray. Regards, Ioan -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Kane, Amol (349) Sent: Tuesday, June 06, 2006 11:18 AM To: [log in to unmask] Subject: [TN] Rework Systems Hi, What rework systems are being used out there for Lead-free component removal and replacement. Who are the reputed vendors in this field and what are your experiences? Thanks in advance Amol Kane Process Engineer Harvard Custom Manufacturing 941 Route 38 Owego, NY 13827 Phone: (607) 687-7669 x349 [log in to unmask] --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------