Ben, The density of pure tin is 7310 kg/m3. We use about a jar per day per SMT line. If a jar is 700 grams it would be 96cc's. We have two lines and are a small shop doing high mix medium volume and we would be burning an EXTRA 324 gallons of gas every 10 days or 11826 gallons per year give or take. Then there's the Wave. Regards, Martin -----Original Message----- From: Gumpert, Ben [mailto:[log in to unmask]] Sent: Tuesday, June 06, 2006 4:00 AM To: [log in to unmask] Subject: [TN] How much solder is 1000 cc? John, I've seen this quote several times now: "The difference between SAC (the replacement solder) and SnPb (the leaded solder) is 453 kg of NRR per 1,000 cc of solder applied. If this were all automotive gasoline, this difference is equivalent to 162 gallons of gasoline." But how much is 1,000 cc of solder? How much solder does the average walkman, cell phone, microwave, etc. contain? Or perhaps a better questions are; how much solder does the average consumer purchase per year or how much solder does the world consume each year? This amount of gasoline becomes less impressive if it is spread over a number of years for a single consumer. Ben -----Original Message----- From: John Burke [mailto:[log in to unmask]] Sent: Thursday, June 01, 2006 4:52 PM Subject: RoHS article in Boston Globe Good morning, I read your article, which was brought to my attention by the members of the technical forum link on the IPC web site so I have copied this to them as they may want to fire in some comments too (or maybe not) We are the people globally that are being impacted by this legislation. The views below are my views and the opinions are backed up by recent scientific data form the US EPA. The RoHS legislation is excellent in every respect but one - taking lead out of solder. Removing lead in solder is and will cause a huge hit to the environment as outlined in a recent US Environmental Protection Agency (EPA) report which states the following: "The difference between SAC (the replacement solder) and SnPb (the leaded solder) is 453 kg of NRR per 1,000 cc of solder applied. If this were all automotive gasoline, this difference is equivalent to 162 gallons of gasoline. Assuming a driver consumes 20 gallons per week, this is also equivalent to approximately 8 weeks of driving" and note that the increased environmental impact is from the "green" replacements. The thought process for lead in solders removal is intuitive. The reality of the result is counter intuitive - removing it is environmentally a bad thing... This sound like a crazy e-mail but the facts speak for themselves all of which can be found by looking at the http://www.rohsusa.com <http://www.rohsusa.com/> site and the blogs at http://www.rohsusa.com/blog which is attracting 300000 hits a month since it was put up to highlight these issues in April. The reality is that the EU did NOT carry out any scientific analysis such as is contained in the EPA report before it brought out this legislation, and the TAC technical advisory committee who deal with exemption requests are not technical. Further, they appear to have dismissed out of hand at least one exemption request put to the EU commission in 2004 on these very environmental grounds without looking into the data. Here is a set of bullet points on the situation and laid out by the front home page of the web site:- 1. Europe has initiated RoHS in isolation (unlike Kyoto or the Montreal protocol) and as such has impacted the global electronics market by an estimated 100 billion dollars. If as a result of this legislation, electronics becomes very unreliable very quickly. I believe that a collective of manufacturers could take the Euro parliament to court and win. 2. Expert opinion says that reliability WILL be an issue and that the replacements for leaded solder are simply not as reliable as their leaded predecessors. As this site grows, I will be providing links and examples of failures if/as they occur. If you have any examples, please email me. 3. The environment is going to be negatively impacted by the changeover to lead free. The numbers are available in the August 2005 EPA report. 4. There is going to be wholesale destruction of non-replaceable forests and other resources as the tin industry continues to struggle to control unauthorized mining of the raw materials. 5. There is not a shred of evidence to suggest that the change was necessary or even desirable from an environmental, health, or engineering standpoint. And please note that this initiative is driven purely by concern for the environment and does not have any financial interest in the outcome either way. Kind regards, John Burke RoHSUSA --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------