Wee Mei, if I understand what you are looking for, it is in several places in the original IPC/WHMA-A-620. Clause 9.4.4 Connector Damage - Contacts <not the most intuitive header> has criteria for inserted connector contacts. In Revision A "damage" and "installation" are separated with installation now Clause 9.5 Clause 13.8 Center Pin Position <coaxial connector section> In Revision A this is now 13.9. 620A 9.5 Installation of Contacts and Sealing Plugs into Connectors Contacts retention (seating/locking) shall be verified with a non-destructive process appropriate to the connector in use, such as visually through an inspection window. Verification shall be accomplished prior to addition of any restraining devices. Unused contact locations shall be filled with contacts and/or plugs if specified on the documentation. The contacts are not crimped unless required for insertion. Exceptions to retention verification include: *Prewired molded connectors. *Potted or molded connectors after molding/potting. *Solder cup connectors. *Connector contact lead ends that are soldered into position. *Connector contact locking device that is visible through an inspection window. Acceptable - Class 1,2,3 *All connector contacts are seated and locked into position. *All locations in connector have been filled (if required). Defect - Class 1,2,3 *Contact is not seated as visible through inspection window. *Pin or socket is not seated and locked. *Contact(s) missing when unused positions are required to be filled. 13.9 Center Pin Position The location of the center conductor's connector contact is critical to meeting the electrical signal's integrity requirements. In the case of "fixed" coaxial cable center conductor contacts, the position of the center contact is determined by the design of the connector, and the assembly process generally minimally affects the position of the center conductor's contact. The position of "Floating" center conductor contacts is greatly affected by the assembly, primarily due to shield termination and wire preparation cut/trim lengths. Refer to manufacturer's assembly specifications. Target- Class 1,2,3 *Center pin fully seated into housing of connector. Defect - Class 1,2,3 *Center pin not fully seated into housing of connector. *Center pin is bent (not shown). *Center pin extends beyond proper height (not shown). Is this the kind of criteria you are looking for? The 620 committee had a teleconference this morning to resolve some comments received during ballot. Rev A will be going out for 2nd 30-day ballot by Friday of this week, publication target early July. Jack Jack Crawford, IOM IPC Director Certification and Assembly Technology [log in to unmask] 847-597-2893 FAX 847-615-5693 3000 Lakeside Drive, Suite 309 S Bannockburn, IL, 60015 -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Lum Wee Mei Sent: Tuesday, May 16, 2006 9:19 PM To: [log in to unmask] Subject: [TN] IPC 620 Hello, I flipped through the whole of IPC 620 but did not find anything about insertion pin height. I remember in the old MIL std, it mentioned that inserted pin must ensure to have level height to consider acceptable. Is this criteria no longer important? The reason I asked is because we come across some connectors have their inserted pins being pulled back into the socket after the wires are tighten. Should it not consider reject? If such connectors with sunken pins are plugged into their mating part, the connectivity will be a problem For your kind advice. Thanks and regards, Wee Mei --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------