Forward it to Technet christian ge <[log in to unmask]> 写道: 日期: Thu, 25 May 2006 10:10:55 +0800 (CST) 发件人: christian ge <[log in to unmask]> 主题: 回复: RE: [TN] Thermal cycle test for plated through holes filled with epoxy ink and cap plated on the top 收件人: "Whittaker, Dewey (AZ75)" <[log in to unmask]> Hello Dewey, The test set-up is -40degree C to +145degree C, 1000 cycles. Dwell time at each temperature is 30minutes. Now the problem is that we see complete barrel crack (i.e length of barrel crack is equal to the plated copper thickness on hole wall) after cross-section. Thanks, Chris. "Whittaker, Dewey (AZ75)" <[log in to unmask]> 写道: Not knowing your test set-up and how accurate your resistance measurements were and any other relevant correlation factors, I couldn't say. However IMHO anything above a 2 % resistance gain is a failure. Varying degrees of barrel cracking will almost always be a reality, but not necessarily a failure when it comes to thermal cycling or other accelerated stress testing. Dewey -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of christian ge Sent: Monday, May 22, 2006 11:53 PM To: [log in to unmask] Subject: [TN] Thermal cycle test for plated through holes filled with epoxy ink and cap plated on the top Hello Technetters, I need your help on the following thermal cycle test problem. Recently we asked our PCB suppliers to do 1000 cycle thermal cycle test for 6L, daisy chain boards with plated through holes filled with epoxy ink and cap plated on the top of the holes( or via-in-pad design). The resistance change before and after thermal cycle test is less than 5%, however the holes have complete barrel crack. Have you seen this kind of problem before? Can I approve the supplier's test result? Here are some more information about the test for your reference. 1) board thickness: 1mm (40mils) 2) hole size: 20mils, 18mils, 15mils, 10mils. All have complet barrel crack except the holes of 10mils . Thanks for your help in advance! Chris __________________________________________________ 赶快注册雅虎超大容量免费邮箱? --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- http://cn.mail.yahoo.com --------------------------------- 抢注雅虎免费邮箱-3.5G容量,20M附件! --------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- 抢注雅虎免费邮箱-3.5G容量,20M附件!