Cheryl: Plating from solutions involves transfering electrons to ions floating in solution, converting them to metals, hopefully on the surface we want. There are three kinds of plating from solutions... immersion plating electroless plating electrolytic plating The three different methods differ in the source of the electrons... In immersion plating, some of the substrate dissolves, releasing electrons, which cause the metal in solution to plate out. This kind of plating is self-limiting, when the substrate material gets covered, plating stops. This is why you cannot get gold over about 0.25 micron in IMMERSION gold. In electroless plating, another chemical in solution donates electrons to the metal ions in solution, causing them to plate out. There is theoretically no limit to the thickness you can achieve using electroless plating... thus achieving 0.5 micron gold can be done with ELECTROLESS gold. And for the record, the rectifier, also known as the "electron pump", pumps electrons from the anode to the cathode in electrolytic plating. Rudy Sedlak RD Chemical Company Cheryl Johnson <[log in to unmask]> wrote: I believe I have seen this somewhere, and have tried searching the archives, but am having trouble finding it. Does anyone know of any processes for electroless gold that can obtain > .5 micron thickness (without needing bus bars?) Or any way to get > .5 micron gold on a flex without bus bars? Thank you! Sincerely, ----------------------------------- Cheryl Johnson, C.I.D.+ Manager ExcelStor US Office, Engineering Services Email: [log in to unmask] Tel: (303) 684-7291 Fax: (303) 684-7268 Mobile: (303) 809-5815 ----------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- Be a chatter box. Enjoy free PC-to-PC calls with Yahoo! Messenger with Voice.