Has anyone run into problems using PCBs with ENIG finish in regular SnPb IR reflow or wave solder processes? I just talked to someone who said that there were industry advisories out from a couple of companies (maybe Intel & Radisys??) advising against that mixture of solder & surface finish, but I have not heard anything about that on either the TechNet or Lead-Free discussion groups, and a Google search for "SnPb solder ENIG finish" didn't turn up any immediate warnings either. Many thanks in advance for any information, -Camille Good Portland, Oreong --------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- Yahoo! Messenger with Voice. Make PC-to-Phone Calls to the US (and 30+ countries) for 2¢/min or less.