Ah, I believe you are trying to remove mask from the pads? If you are doing this on enig boards be advised that you will also have to "finish" them with Entec as you will expose bare copper if that is the case. John -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Kevin Glidden Sent: Monday, May 08, 2006 7:09 AM To: [log in to unmask] Subject: [TN] Laser Ablation of Soldermask Hi all, We have lasers available to us in house, used for other processes, but I am wanting to use these lasers for laser ablation of solder mask on our PCBs. I am new to the laser process and operation, but have experienced technicians to rely upon. Any general or specific advice in terms of intensities, speed, or other factors? Thanks, Kevin --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------