Steven I would be careful about electrolytic silver in electronic applications. While this has not been a problem with immersion silver there have been problems with silver migration using electrolytic silver. Most likely, because the silver inventory is increase many times over. Best regards Lee J. L. Parker Ph.D. JLP Consultants LLC (804) 779 3389 -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Creswick, Steven Sent: Wednesday, May 24, 2006 3:00 PM To: [log in to unmask] Subject: [TN] Electrolytic Ag Suppliers for COB applications All, I do not wish to get any plating bath suppliers in trouble by responding to the forum at large [and come across as selling themselves], but if there is anyone lurking out there in the bushes that knows of a plating bath supplier selling electrolytic Ag for gold wire bonding applications, please contact me directly. I am speaking of automotive type quantities, but can not really get into the application. The underlying nickel could be electroless or electrolytic. Would like US and overseas users of said bath/s if possible. Have checked the archives, but did not locate appropriate info Steven Creswick Gentex Corporation 616 772 1590 x846 --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------