I hope it is extremely close to Sn63Pb37 at 220. Kerry McMullen Principal New Product Mfg. Engineer LTX Corporation 50 Rosemont Road Westwood, MA 02090-2306 (T) 781-467-5468 "David D. Hillman" <[log in to unmask]> Sent by: TechNet <[log in to unmask]> 05/02/2006 11:32 AM Please respond to TechNet E-Mail Forum <[log in to unmask]>; Please respond to [log in to unmask] To [log in to unmask] cc Subject [TN] Surface Tension Data for SAC305 Hi TechNet land! Hey, need some speedy assistance - the JSTD-002 and JSTD-003 committees need a piece of technical data. We are looking for the surface tension of SAC305, in J/m2, at 255C. Anyone who can supply that value will win a large chocolate ice cream cone from Dairy Queen courtesy of me at the next IPC meeting! TIA! Dave Hillman JSTD-002/003 Chairman [log in to unmask] --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------