Conversion to RoHS may or may not have a large impact on your PCB function. As to your specific scenario, I would expect some performance impact due to Nickel being a RF barrier metal. You may want to look at an Immersion Silver (IAg) that can actually have a performance improvement over HASL. I would suggest you also look at the material you are using to assure there are no concerns of higher temp degradation. You may find just changing finish is enough, or you may need to update your circuit for newer materials and finishes. Good Luck, FNK Frank N Kimmey CID+ Principal PCB Designer Powerwave Technologies Inc Office 916-941-3159 Fax 916-941-3195 Cellular 916-670-0645 -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Selva Suganthi Sent: Thursday, April 06, 2006 5:44 AM To: [log in to unmask] Subject: [TN] Regd Rohs Conversion - didn't get any reply!!! Dear All, Whats the impact for Rohs conversion on PCB? Will the conversion affects the characteristic impedance of the board? The situation is as follows My Board has a RF antenna trace with some grounding vias. We are trying to convert from HAL finishing to GOLD Flash? will this conversion affect the impedance of RF antenna trace? Thanks and Regards Suganthi --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------