Hi, Edding 8404 aerospace marker remains and is resistant also to conformal coating materials. b.r. Jarmo Schaefer, Chris wrote: > Hello all, > > Can anyone tell me where I can get single part epoxy pens? I am looking for a way to mark FR4 (on the dge) CCA's to indicate operations have been performed, but everything I have tried washes off in the inline cleaner. We are using a Kyzen A4520 at 15% concentration 125F and everything we try comes off. So our last resort is to go with single part fast cure epoxy and hopefully be able to get it in different colors and in a form that allows us to put it on quickly and easily. > > Please help obi whan kenobie your my only hope. Its almost Friday - getting a little excited. > > Thanks in advance. > > Chris Schaefer > Suntron Corporation > Process Engineer > 540 N. Rogers Road > Olathe, Kansas 66062 > 913.393.5878 > [log in to unmask] > > NOTICE: > > This message is intended for the use of the individual entity to which it is addressed and may contain information that is privileged, confidential and exempt from disclosure under applicable law. If the reader of this message is not the intended recipient, or the employee or agent responsible for delivering the message to the intended recipient, you are hereby notified that any dissemination, distribution or copying of this communication is strictly prohibited. If you have received this communication in error, please notify us immediately by calling 913.393.5878 or returning the original message to us. > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 1.8e > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 > ----------------------------------------------------- > > --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------