True, but it these tests results came from a study where the solder stencil had been optimized for knowing the attributes of the board. In the CM world these things have a way of dropping in on us. The arithmetic is not complex, but it is also not a no-brainer. -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Leo Higgins Sent: Monday, April 24, 2006 4:52 PM To: [log in to unmask] Subject: Re: [TN] Solder joint reliability of BGAs and 0402 chip on blind vias Some work has been published actually showing better mechanical shock / drop test results for unfilled via-in-pad solder pad structures, even with the common presence of a void in the solder located right in the recessed via. This helps avoid the issue of lifted copper that is often seen over the top of filled microvias. Best regards, Leo Leo M. Higgins III, Ph.D. Vice President, Technical Operations ASAT, Inc. 3755 Capital of Texas Highway, Suite 100 Austin, Texas 78704 -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Bob Wilson Sent: Friday, April 21, 2006 1:11 PM To: [log in to unmask] Subject: Re: [TN] Solder joint reliability of BGAs and 0402 chip on blind vias Yup. Laser drill at 4 mil diameter and fill with good conductive epoxy. When I hooked the board up I eased the fabrication a bit by doing the blinds only from layer 1 to layer 2 and layer 15 to layer 16. (Layers 2 and 15 were flooded GND planes). Boards were fabbed at Hallmark Circuits in San Diego. I talked to them before I routed a signal and the boards worked fine. Bob Wilson CID -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Ted Kong Sent: Friday, April 21, 2006 10:57 AM To: [log in to unmask] Subject: [TN] Solder joint reliability of BGAs and 0402 chip on blind vias Hi all, Has anyone used blind vias on BGAs or 0402 chip packages? Will they form reliable solder joints? Thanks all in advance. Ted __________________________________________________ Do You Yahoo!? Tired of spam? Yahoo! Mail has the best spam protection around http://mail.yahoo.com --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------