According to a plating Guru, ImSn includes some organic components in the Tin plating that relaxes the stress. That may explain the mitigating or elimination of whiskers. The plating is done electro less in a chemical plating soup up to 0.05 mils or 50 millionths thickness. This may be the way to go to eliminate or minimize whiskers on component terminations. Ramon -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D. Sent: Thursday, March 16, 2006 5:16 PM To: [log in to unmask] Subject: [TN] FW: [TN] Immersion Tin Specification -----Original Message----- From: Stadem, Richard D. Sent: Thursday, March 16, 2006 4:12 PM To: 'Vladimir Igoshev' Subject: RE: [TN] Immersion Tin Specification My apologies, Vladimer. I double checked my information. I have a finish provider whose documentation for a bright tin finish on the PWB claims it is "whisker-free". That confused me. I went back over the references I have (NEMI report and "Tin Whiskers: Attributes and Mitigation" by J. Brusse, G. Ewell and J. Siplon, and other references)and they support what you are saying. The finish vendor apparently recommends putting the bright tin over a nickel base, which supposedly mitigates the whisker formation. Does this make sense? There is so much conflicting information amongst those providing tin finishes for components versus tin finishes for circuit boards it is hard for me to keep it all straight. -----Original Message----- From: Vladimir Igoshev [mailto:[log in to unmask]] Sent: Thursday, March 16, 2006 3:52 PM To: Stadem, Richard D. Subject: Re: [TN] Immersion Tin Specification Richard, Can you send me the referrence? Unless I'm completely confused, that is not what I've been hearing. Vladimir Sent from my Blackberry Wireless Vladimir Igoshev, 519-888-7465 ext.5283 ----- Original Message ----- From: Stadem, Richard D. <[log in to unmask]> To: Vladimir Igoshev Sent: Thu Mar 16 16:47:42 2006 Subject: RE: [TN] Immersion Tin Specification Thank you. Then why is it reported that matte tin has a greater tendency to incur tin whiskers? Would it be because of a higher stress factor in the grain? -----Original Message----- From: Vladimir Igoshev [mailto:[log in to unmask]] Sent: Thursday, March 16, 2006 3:43 PM To: [log in to unmask]; Stadem, Richard D. Subject: Re: [TN] Immersion Tin Specification As far as I know, immersion tin is better than mette and of cause bright ones Vladimir Sent from my Blackberry Wireless Vladimir Igoshev, 519-888-7465 ext.5283 ----- Original Message ----- From: TechNet <[log in to unmask]> To: [log in to unmask] <[log in to unmask]> Sent: Thu Mar 16 16:39:34 2006 Subject: Re: [TN] Immersion Tin Specification Better than what? Better than it used to be? Could you clarify, as I am wondering what you mean by that. Thanks. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Vladimir Igoshev Sent: Thursday, March 16, 2006 3:29 PM To: [log in to unmask] Subject: Re: [TN] Immersion Tin Specification Ramon, Immersion Tin is MUUUUUCH better in terms of whiskering. Vladimir Vladimir Igoshev, Ph. D. Manager, Metallurgical Lab Research in Motion 451 Phillip St. Waterloo, ON, N2L 3X2 Voice: (+1) 519-888-7465, ext. 5283 Fax: (+1) 519-886-0863 E-mail: [log in to unmask] -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Dehoyos, Ramon Sent: Thursday, March 16, 2006 4:12 PM To: [log in to unmask] Subject: Re: [TN] Immersion Tin Specification John: Just curious, what is the tin plating going to be used on? Thin Tin plating produces whiskers, which can be a nightmare. Thicker Tin plating helps as a whisker mitigating factor. These whiskers have shot down a nuclear power plant and caused space craft failures. Tin plating can very problematic. Whiskers can grow in days or take years. Regards, Ramon -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of R Sedlak Sent: Thursday, March 16, 2006 4:01 PM To: [log in to unmask] Subject: Re: [TN] Immersion Tin Specification John: Generally accepted goal is one micron, or 40 microinches, thickness. You essentially never have to worry about it being too thick, and thickness of less than 75% of that value should raise eyebrows... Rudy Sedlak RD Chemical Company John Parsons <[log in to unmask]> wrote: IPC have graciously provided us (the industry) with specifications for ENIG (IPC-4552) and Immersion Silver (IPC-4553), is there a similar specification Immersion Tin (white tin)? If not, is there a generally accepted specification for material thickness? John Parsons --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------- Brings words and photos together (easily) with --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- PhotoMail - it's free and works with Yahoo! Mail. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------------------------- This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------------------------- This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful. --------------------------------------------------------------------- This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------