"ID" - DP There are a lot of issues to consider, like how easy the flux is to remove, how effective the cleaning process is, and what kind of flux traps are present in the design. So you have to test. J-STD-001 gives you the goods. In Rev. C it's Appendix B, and in Rev. D it's Appendix C. When we qualified our process, we performed SIR and ion chromatography, plus a few other things. Joe Kane BAE Systems Johnson City, NY -----Original Message----- From: Donald Vischulis [mailto:[log in to unmask]] Sent: Thursday, March 09, 2006 5:59 PM To: [log in to unmask] Subject: [TN] Cleaning Qualification Question All I've been assigned the task of determining if a supplier's current cleaning process is robust or if additional testing is required to be able to say that the product is clean enough to provide years of field use. The board is a 2-sided Class 3 assembly (95% SMT) with one BGA and about 1500 other components. The assembly is soldered with a water soluble flux, it's cleaned in a batch cleaner with DI water, and is conformal coated. The current manufacturer is using and Omega meter to verify the cleanliness of the board after cleaning. My questions: Is this process good enough to provide a reliable product in an aircraft application? If not what guidance is available to determine what level of process qualification is needed to answer question #1? Any help is really appreciated. Don Vischulis --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------