IPC 610 Rev D ( 8.2.5.4???) Side Fillet is by length and evidence of wetting, no height. The reason you cannot find a toe requirement is that there is not one. Components often have a pre-plated cropped end so it isn't necessarily wettable. You are also allowed toe overhang of the pad. Rex -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of sumxp Sent: 06 February 2006 15:23 To: [log in to unmask] Subject: Re: [TN] Gull wing side & toe fillet height Sorry,I am referring to side and toe fillet Height. Thanks sumxp --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ________________________________________________________________________ This email has been scanned for all viruses by the MessageLabs SkyScan service. ________________________________________________________________________ This email has been scanned for all known viruses by the MessageLabs SkyScan service. ================================================================ This email (including any attachments) is confidential and/or may be legally privileged. It is intended for the named recipient (s) only and may not be forwarded, disclosed or otherwise disseminated Although this email has been scanned for viruses, WE DO NOT (to the extent permitted by law) ACCEPT ANY LIABILITY WHATSOEVER for any virus infection, compromise of security or losses resulting from vi NO CONTRACT MAY BE FORMED OR DOCUMENTS SERVED BY THIS EMAIL unless specifically agreed to in writing and signed by a Director of Hansatech. Any views or opinions expressed in this email are those of If you have received this email in error please contact the IT department immediately on (01202) 674 333 or (01553) 691 022 prior to deletion. ================================================================ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------