Hi Dominic You could try Speedprint at Europlacer, it also depends what printer you are using. We use a speedprint 200 and the pressure is .06kg and the speed is 110m/sec but again a lot depends on your stencil as well. Regards Stuart DCC Electronics -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Dominic Boudreau Sent: 06 February 2006 16:10 To: [log in to unmask] Subject: [TN] solder paste printing process Hello, We are trying to control our solder paste printing process and I want to know if someone knows good links about this subject. Specifically, I am looking about: - How to set the printer parameters (squeegee speed, pressure, etc...) - Solder paste deposit inspection Thanks Dominic --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------