Others have responded that the cost of immersion silver is usually much less than ENIG. But what you need to consider also is whether to use the nickel with flash gold, standard electroless nickel/immersion gold (ENIG), or immersion silver. When soldering to the immersion silver finish the silver will be absorbed into the solder and the solder joint will be formed on copper. With the flash gold over nickel or the ENIG plating the gold will be absorbed into the solder and you will form a solder joint to the nickel. Either of the flash gold over nickel or ENIG requires plating of nickel, and as such the process is susceptible to nickel skips, which you have already experienced. Not much fun. The solder joints formed on copper will be stronger than those formed on nickel because of nickel's much slower rate of dissolution into the solder joint. Because of the slower dissolution rate, the assembly requires more heat, and for a longer time, especially under the BGAs. BGAs do an excellent job of insulating the solder spheres. If you have BGAs or chip scale components, you will be much better off with immersion silver finish on the PWB. If you have high impedance/high frequency circuitry you will also be much better off with immersion silver. Buy a sample of boards and qualify the assembly with the different plating no matter which one you choose. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Sumxplore Sent: Friday, January 13, 2006 11:55 PM To: [log in to unmask] Subject: Re: [TN] enig bad board Looks like this is the beginning of my nightmare with more to come after reading those valuable feedback by technetters. No,I haven't try immersion silver but certainly I will explore it.Anyone can let me what is the cost differences between Immersion silver and ENIG? Thank you. ----- Original Message ----- From: "Lee Parker" <[log in to unmask]> To: "'TechNet E-Mail Forum'" <[log in to unmask]>; "'sumxp'" <[log in to unmask]> Sent: Saturday, January 14, 2006 1:34 AM Subject: RE: [TN] enig bad board > Sumxp > > It is likely the thickness of the gold is inadequate and the > underlying nickel has oxidized. I would measure the gold thickness > (XRF) and compare it to the minimum specified. The silver color after > erasing is most likely the nickel that is under the gold and with the oxides removed. > > There are many other alternatives these days to ENIG such as immersion > silver. Have you evaluated into any of these? > > Best regards > > Lee > > J. L. Parker Ph.D. > JLP Consultants LLC > (804) 779 3389 > > > Best regards > > Lee > > J. L. Parker Ph.D. > JLP Consultants LLC > (804) 779 3389 > > > -----Original Message----- > From: TechNet [mailto:[log in to unmask]] On Behalf Of sumxp > Sent: Friday, January 13, 2006 10:48 AM > To: [log in to unmask] > Subject: [TN] enig bad board > > Hi, > > We noticed few ENIG bga pads black in color instead of gold.It turn > silver when use eraser to remove away the black color pad.What is the > defect mode? > Any reliability issue?Is it advisable to continue using these pcbs? > > Thanks...... > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 1.8e To > unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt > or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing > per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: > http://listserv.ipc.org/archives Please visit IPC web site > http://www.ipc.org/contentpage.asp?Pageid=4.3.16 > for additional information, or contact Keach Sasamori at > [log in to unmask] or 847-615-7100 ext.2815 > ----------------------------------------------------- > R > > > -- > No virus found in this incoming message. > Checked by AVG Anti-Virus. > Version: 7.0.344 / Virus Database: 267.14.17/228 - Release Date: > 1/12/2006 > > --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------