be careful what you wish for: (a) if you use reliability test chamber, your QA will kill you (can't clean it up enough to next rel test). (b) if you use accelerated cure, some of RTV will be extra hard compare to the room temp 7 day process... what ever you qualed before, may not be valid if you change the cure procedure. jk -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Kevin Glidden Sent: Monday, January 23, 2006 9:40 AM To: [log in to unmask] Subject: [TN] Humidity Cure Chambers Hi all, Does anyone know where I can look for simple humidity chambers for curing moisture-cure RTV? My searches yield all programmable, temperature / humidity chambers, which is a little overkill for what I need. All I need is steady-state humidity @ 50% RH with only slight warming above room temperature - 80F or so. We are currently using a wooden box with a light bulb or two and a bowl of water. Doesn't seem like the best solution, but perhaps it is? Thanks in advance, Kevin --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------