Hi Bill - Just to give you a short background, Rockwell Collins utilizes all of the immersion finishes - immersion tin, immersion silver and ENIG - in our avionics designs depending on the use environment conditions. So we have had the "opportunity" to see the good, the bad, and the ugly for each of the finishes. Immersion silver has traditionally had two disadvantages: a) silver is a very reactive element so many folks have corrosion concerns; b) silver is a very reactive element so surface changes are very apparent. The IPC committees have done some extensive work demonstrating that a correctly applied immersion silver surface finish is equal to or better than tin/lead in many (but not all) use environments. There are some use environments that will cause problems - direct/constant exposure to a marine environment would be one example - but overall ImAg is pretty robust. Silver oxides is as conductive as elemental silver (which is a very cool characteristic in the metal's world) and are very solderable. Silver chloride and silver sulfide are the two surface species that can cause issues. My packaging issue comment relates to those two species - if you don't package ImAg pwbs using some type of "anti-tarnishing" paper or don't strictly control your pwb storage conditions then you risk the issue of having the tarnish issues. A little tarnish on the surface isn't a killer - most flux systems deal with it quite well and good solder joints are possible. But if you get a heavy black tarnish then the pwb solderability is an issue. Don Cullen and the MacDermid folks have published a couple of studies demonstrating the impact of ImAg tarnish on solderability. And there is an IPC committee currently working on a PWB Handling/Storage guidelines document to aid the industry in this area. Hope this helps- good luck on your investigation. Dave Hillman Rockwell Collins [log in to unmask] [log in to unmask] Sent by: TechNet <[log in to unmask]> To [log in to unmask] cc 01/24/2006 06:26 PM Subject Re: [TN] Immersion Gold and LF PROCESS Please respond to TechNet E-Mail Forum <[log in to unmask]> ; Please respond to [log in to unmask] To Dave: What specific packaging issues are there for Immersion Silver??? My company may be heading in this direction!!!!! Thank in advance for your inputs!!!!! Bill Black Q.A.Mgr. Medco --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------