Dear Ramon But most of the manufacturer can not succedd in full joint soldering , and it is normal for them to touch up after assembly and they may indicate some ppm value according to their experience but we just want to support our claims based on writen or accepted criteria or standard. We also want to reach a point where there is no nonwetting opportunity but sometimes some of the pads or soldering region need to be touched up or reworked after assembly Best Regards Yusuf Dehoyos, Ramon yazmış: > > Hi Les: > I agree, six sigma is achievable, if you have dedicated personnel, tech support and standardized good equipment that work in a symbiotic relationship. It is hard but it can be done. Toyota manufacturing plants are doing just that even in the U.S. Ego gets in people's way and prevents that from happening. It is a shame. Some people are more preoccupied in bettering themselves than moving the company forward as a whole. Do you know the DPMO to be six sigma? > Regards, > Ramon > > > > _____ > >From: - Bogert [mailto:[log in to unmask]] >Sent: Monday, December 05, 2005 5:34 PM >To: TechNet E-Mail Forum; Dehoyos, Ramon >Subject: Re: [TN] Nonwetting Pad numbers > > >But it is not six sigma. > > ----- Original Message ----- > From: Dehoyos, Ramon <mailto:[log in to unmask]> > To: [log in to unmask] > Sent: Monday, December 05, 2005 1:16 PM > Subject: Re: [TN] Nonwetting Pad numbers > > Less than 1000 defects per million ops is good, less than 500 DPMO is great. > Regards, > Ramon > > > > -----Original Message----- > From: TechNet [mailto:[log in to unmask]] On Behalf Of Brooks,Bill > Sent: Monday, December 05, 2005 1:07 PM > To: [log in to unmask] > Subject: Re: [TN] Nonwetting Pad numbers > > Yusuf Gomec, > > This is a strange question from a designer's point of view... If you send me a board with "nonwetted or insufficient soldered pads" we will reject them. > 100% of all solder locations must be properly soldered, all the time, every day, no exceptions. There is no criteria for 'acceptable numbers' for bad solder joints. The circuit will not work or be reliable unless they are all good solder joints. You cannot tolerate bad solder or dewetted surface finishes. > > Now... if you are looking for statistical figures for the industry about how much scrap or rework assembly houses make, someone else will have to answer that one... Although it occurs to me that data might be a point of interest to someone trying to set up or run a board shop and figure out the costs of doing business... > > Your company BaskiDevre is in the business of making boards is it not?... I would expect that your Quality Assurance people would have collected this statistic and it would be used as a running gauge for seeing if they had control of their processes and were maintaining them correctly in order to keep those numbers as small as possible with the equipment and methods that they had to work with. The ideal situation would be zero defects, like John Burke says. That would mean your process controls were working. > > Best regards, > > Bill Brooks - KG6VVP > PCB Design Engineer, C.I.D.+, C.I.I. > Tel: (760)597-1500 Ext 3772 Fax: (760)597-1510 Datron World Communications, Inc. > _______________________________________ > San Diego Chapter of the IPC Designers Council Communications Officer, Web Manager http://dcchapters.ipc.org/SanDiego/ > http://pcbwizards.com > > -----Original Message----- > From: Baski Devre [mailto:[log in to unmask]] > Sent: Monday, December 05, 2005 9:05 AM > To: [log in to unmask] > Subject: Re: [TN] Nonwetting Pad numbers > > I may ask wrongly so please let me ask again. What is the ppm of nonwetted or insufficient soldered pads numbers which will be touched up after assembly of the PCBs > > John Burke yazmýþ: > > >That would be zero > >john > >Sent with Wireless Sync from Verizon Wireless > > > >---- Original Message ---- > >From: "Baski Devre" <[log in to unmask]> > >Date: 12/5/05 8:42 am > >To: "[log in to unmask]" <[log in to unmask]> > >Subj: [TN] Nonwetting Pad numbers > >Dear Technetters > >What are the acceptibility criteria of nonwetting PCB for a PCB which > >has about thousand pads both smd pads and through hole pads.holes . > >Or, is there any standard which can state that after assembly how many > >pads are tolerant to not being soldered per 1,000 pads. > >Best Regards > > > > > > > > -- > Yusuf GÖMEÇ > Product Quality Engineer > > BASKI DEVRE SAN ve TIC LTD STI > Ceyhan Sk. No:10 34896 Pendik-Istanbul-Turkey > > Tel: 00 90 216 3901036 (4 Hat/Line)-173(Extention) > 00 90 216 4836560 (4 Hat/Line)-173(Extention) > Fax: 00 90 216 3544941 > 00 90 216 4913269 > Gsm: 00 90 533 6579897 > 00 90 533 7480014 > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 > for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 > ----------------------------------------------------- > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 > ----------------------------------------------------- > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 1.8e > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 > ----------------------------------------------------- > > > >--------------------------------------------------- >Technet Mail List provided as a service by IPC using LISTSERV 1.8e >To unsubscribe, send a message to [log in to unmask] with following text in >the BODY (NOT the subject field): SIGNOFF Technet >To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) >To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest >Search the archives of previous posts at: http://listserv.ipc.org/archives >Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 >----------------------------------------------------- > > > -- Yusuf GÖMEÇ Product Quality Engineer BASKI DEVRE SAN ve TIC LTD STI Ceyhan Sk. No:10 34896 Pendik-Istanbul-Turkey Tel: 00 90 216 3901036 (4 Hat/Line)-173(Extention) 00 90 216 4836560 (4 Hat/Line)-173(Extention) Fax: 00 90 216 3544941 00 90 216 4913269 Gsm: 00 90 533 6579897 00 90 533 7480014 --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------