Susan, I would hope the customer would spec out the laminate as RoHS compliant, high Tg and from this the Fabrication house should infer the board will be used in a lead-free process. Sadly, some fab houses/end users think that the old standard FR4, if plated with ENIG or IAg is RoHS compliant and therefore can be used in a lead-free process. Too bad our esteemed membership does not make up all the specifiers of materials. If that were the case this would all be a moot point. My 0.5 rubles. Phil -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Susan Mansilla Sent: Tuesday, December 13, 2005 10:13 AM To: [log in to unmask] Subject: Re: [TN] Qualification of the Pb-free capable manufacturers Greetings to All One aspect of this is when to test. I do understand Werner's desire to have the raw material tested in some way to determine if it has the needed ppm/C - but I am still concerned about a multilayer board and the need to test it in some way to see if it has been cured sufficiently/has appropriate adhesion enhancement between layers etc to meet the needed ppm/C. The same questions then become what to test and how to test? The 6012 group is meeting in Mesa in January and some of the topics are how and what need adjustments when LF applies. The other puzzle is when will a fabricator know that the board they make is to be assembled in a LF process. Any suggestions or recommendations are welcome Susan Mansilla Robisan Lab --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------