I do appreciate the acknowlegement of a great role PCB design plays for the output of overall solder quality. To reinforce what is stated here; For last 2 decades, it has been "make it believe" dreams to produce 4 / 6 sigma level quality when PCB designs only meet 2 / 3 sigma level quality. If a design does not meet IPC Class 3, the assembly is not expected to meet the Class 3 quality. What usually ends up doing is that assembly processes are bastardized in the hope of meeting a desirable sigma level or meeting on-time delivery. On top of this, thousands of parts, materials, equipment and processes come into play to produce a desirable sigma level quality that is expected. From my personal thoughts & experience, 50% of PCB assembly defects originate from design aspect, 30% from parts & process materials and 20% from assembly processes. One key point is that understanding manufacturing capabilities and implementing designs to meet the manufacturing capabilities will go a long way to improve DPMO. Thanks Matthew S. Park, Process Development Engineer Vansco Electronics email: [log in to unmask] gtel: (309)-263-7788 dtel: (309)-266-2288 fax: (309)-266-6674 1651 N. Main Morton. IL 61550 >>> [log in to unmask] 12/7/2005 10:56:56 AM >>> And...another aspect of the equation is that the assembly house does not actually have complete control over the soldering statistics... It might not be obvious at first glance but built into those numbers is a dependence upon how well the PCB Designer does their job of providing correct land geometries, component spacing, thermal relief, and planning for copper distribution, etc., this has a big effect on their successful soldering numbers. The particular design being built really plays a large roll in the success of the assembly house in getting all the solder joints soldered correctly on all the boards they build and the assembly engineers are challenged daily to come up with ways to overcome deficiencies in design and 'make' the assembly work. My hat is off to the folks who make their living overcoming difficult design driven assembly problems on a daily basis... you guys and gals are 'wizards' in your own right. The more training we get as designers on how to make their lives easier the better the statistics will be as well. Best regards, Bill Brooks - KG6VVP PCB Design Engineer, C.I.D.+, C.I.I. Tel: (760)597-1500 Ext 3772 Fax: (760)597-1510 Datron World Communications, Inc. _______________________________________ San Diego Chapter of the IPC Designers Council Communications Officer, Web Manager http://dcchapters.ipc.org/SanDiego/ http://pcbwizards.com -----Original Message----- From: Stadem, Richard [mailto:[log in to unmask]] Sent: Wednesday, December 07, 2005 5:06 AM To: [log in to unmask] Subject: Re: [TN] Nonwetting Pad numbers Both of those were excellent responses, Rainer! -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Blomberg, Rainer (FL51) Sent: Tuesday, December 06, 2005 8:59 AM To: [log in to unmask] Subject: Re: [TN] Nonwetting Pad numbers I believe you are asking if there are written or accepted levels of solder touch-up. No, there is no written or accepted level of soldering defects prior to normal touch-up. We all have different "normal" levels of touch-up and all strive for six-sigma values. Differences in design, component type and innumerable other variables drive success. You must support your claims based on your own experience and product and decide what is acceptable for you. > Rainer G. Blomberg > Honeywell -Space Systems Clearwater > Staff Production Engineer (727) 539-5534 -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Baski Devre Sent: Tuesday, December 06, 2005 8:52 AM To: [log in to unmask] Subject: Re: [TN] Nonwetting Pad numbers Dear Ramon But most of the manufacturer can not succedd in full joint soldering , and it is normal for them to touch up after assembly and they may indicate some ppm value according to their experience but we just want to support our claims based on writen or accepted criteria or standard. We also want to reach a point where there is no nonwetting opportunity but sometimes some of the pads or soldering region need to be touched up or reworked after assembly Best Regards Yusuf Dehoyos, Ramon yazmis: > > Hi Les: > I agree, six sigma is achievable, if you have dedicated personnel, tech support and standardized good equipment that work in a symbiotic relationship. It is hard but it can be done. Toyota manufacturing plants are doing just that even in the U.S. Ego gets in people's way and prevents that from happening. It is a shame. Some people are more preoccupied in bettering themselves than moving the company forward as a whole. Do you know the DPMO to be six sigma? > Regards, > Ramon > > > > _____ > >From: - Bogert [mailto:[log in to unmask]] >Sent: Monday, December 05, 2005 5:34 PM >To: TechNet E-Mail Forum; Dehoyos, Ramon >Subject: Re: [TN] Nonwetting Pad numbers > > >But it is not six sigma. > > ----- Original Message ----- > From: Dehoyos, Ramon <mailto:[log in to unmask]> > To: [log in to unmask] > Sent: Monday, December 05, 2005 1:16 PM > Subject: Re: [TN] Nonwetting Pad numbers > > Less than 1000 defects per million ops is good, less > than 500 DPMO is great. > Regards, > Ramon > > > > -----Original Message----- > From: TechNet [mailto:[log in to unmask]] On Behalf Of Brooks,Bill > Sent: Monday, December 05, 2005 1:07 PM > To: [log in to unmask] > Subject: Re: [TN] Nonwetting Pad numbers > > Yusuf Gomec, > > This is a strange question from a designer's point of view... > If you send me a board with "nonwetted or insufficient soldered pads" we will reject them. > 100% of all solder locations must be properly soldered, all the time, every day, no exceptions. There is no criteria for 'acceptable numbers' for bad solder joints. The circuit will not work or be reliable unless they are all good solder joints. You cannot tolerate bad solder or dewetted surface finishes. > > Now... if you are looking for statistical figures for the > industry about how much scrap or rework assembly houses make, someone else will have to answer that one... Although it occurs to me that data might be a point of interest to someone trying to set up or run a board shop and figure out the costs of doing business... > > Your company BaskiDevre is in the business of making boards is > it not?... I would expect that your Quality Assurance people would have collected this statistic and it would be used as a running gauge for seeing if they had control of their processes and were maintaining them correctly in order to keep those numbers as small as possible with the equipment and methods that they had to work with. The ideal situation would be zero defects, like John Burke says. That would mean your process controls were working. > > Best regards, > > Bill Brooks - KG6VVP > PCB Design Engineer, C.I.D.+, C.I.I. > Tel: (760)597-1500 Ext 3772 Fax: (760)597-1510 Datron World Communications, Inc. > _______________________________________ > San Diego Chapter of the IPC Designers Council Communications Officer, Web Manager http://dcchapters.ipc.org/SanDiego/ > http://pcbwizards.com > > -----Original Message----- > From: Baski Devre [mailto:[log in to unmask]] > Sent: Monday, December 05, 2005 9:05 AM > To: [log in to unmask] > Subject: Re: [TN] Nonwetting Pad numbers > > I may ask wrongly so please let me ask again. What is the ppm > of nonwetted or insufficient soldered pads numbers which will be > touched up after assembly of the PCBs --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------