I am not familiar with the P/N 38999 connector yet you speak of a spacer which stirs the mind. Can you share a photo of the animal you are talking about and the spacer application with vertical fill anomaly. Victor, -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Kane, Joseph E (US SSA) Sent: Monday, November 14, 2005 10:47 AM To: [log in to unmask] Subject: [TN] Agilent 5DX Service One of our boards has a number of 38999 connectors, with connections on the top side hidden by a spacer. We've had one SJ failure because of inadequate solder fill up through the PTH. We'd like to determine whether this is an isolated problem, or whether the spacer might be impeding solder flow. Of course, we don't have any boards to sacrifice, and we can't see anything with direct transmission x-ray because the connector is in the way. Anyone know of a lab somewhere nearby that offers scan beam laminography service? Joe Kane BAE Systems Johnson City, NY --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------