Try PEEK It is a plastic that has strength of metals like copper. -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of David Tremmel Sent: Friday, November 11, 2005 1:20 PM To: [log in to unmask] Subject: [TN] High temp material Hello all, Would anyone recommend a high-temp material that can: Be machined for various fixtures and chucks Can withstand lead-free oven profiles Be used for 100 or more thermal cycles and still maintain its form (down to 1mil tolerance) Does not absorb too much heat (compared to a metal) Thank you in advance, David _________________________________________________________________ MSN Latino: el sitio MSN para los hispanos en EE.UU. http://latino.msn.com/ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------