Haven't seen the photos posted yet. But a few questions come to mind... How many metal layers in the flex? Is it circumferential cracking? Where in the via is the cracking occuring? At the knee, in the center, at an innerlayer post interconnec, or...? Is the cracking associated w/ a visible mfg defect in drill quality or plating? dw At 07:03 AM 11/29/2005, Werner Engelmaier wrote: >Hi Mumtaz, >Not having seen pictures, I am reduced to guessing. particularly since you >did not say how thick the flex circuit is. >But when you get copper cracking, it always means that the ductility and >strength of the Cu was insufficient for the loading conditions. Thus, >there are 3 >possibilities alone or in combination: >(1) the properties of the copper deposit are bad; >(2) the loads [thermal expansion, bending, etc] are too high; >(3) geometric stress concentrations create loading conditions too severe for >the available material properties. >A good root-cause-analysis can give you the answer of the causes, which then >allows you to improve the situation as needed. > >Regards, >Werner Engelmaier >Engelmaier Associates, L.C. >Electronic Packaging, Interconnection and Reliability Consulting >7 Jasmine Run >Ormond Beach, FL 32174 USA >Phone: 386-437-8747, Fax: 386-437-8737, Cell: 386-316-5904 >E-mail: [log in to unmask], Website: www.engelmaier.com > > >--------------------------------------------------- >Technet Mail List provided as a service by IPC using LISTSERV 1.8e >To unsubscribe, send a message to [log in to unmask] with following text in >the BODY (NOT the subject field): SIGNOFF Technet >To temporarily halt or (re-start) delivery of Technet send e-mail to >[log in to unmask]: SET Technet NOMAIL or (MAIL) >To receive ONE mailing per day of all the posts: send e-mail to >[log in to unmask]: SET Technet Digest >Search the archives of previous posts at: http://listserv.ipc.org/archives >Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 >for additional information, or contact Keach Sasamori at [log in to unmask] or >847-615-7100 ext.2815 >----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------