Solid P/G layers or solid power / ground planes do not adhere to epoxy glass ( more pockets for moisture ) as well as epoxy glass to another layer of epoxy glass. The more contacts of the same glass to glass the stronger the bond. FR4 with solder mask over the outside layer is tough and will not delaminate easily when properly manufactured. It really can take a lot of abuse. I have seen other materials that are very delicate. They need to be baked at 215 deg C for 4 hours prior to wave solder or there will be delamination. Regards, Ramon -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier Sent: Thursday, October 20, 2005 9:26 AM To: [log in to unmask] Subject: Re: [TN] More on Delamination Hi Steve, I do not think you can make that assumption--the moisture absorption will be pretty uniform after a couple of days. The problem is more with solid P/G layers on dry baking, where more moisture remains near the middle of the PWB. Werner --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------