John, Your assy can probably be reflowed. I would suggest using ENIG as the finish for your bars and PCB. You should then be able to solder using Sn97Ag3 in either a convection with modified profile or a conduction oven. Make sure you are using high Tg/Td materials for the PCB (will need to with stand multiple excursions to ~245C). You will likely need to fixture for second RoHS reflow of components, but this should be the easy part. Call me if you want to discuss off line. Hope it helps, FNK Frank N Kimmey CID+ Principal PCB Designer Powerwave Technologies Inc Office 916-941-3159 Fax 916-941-3195 Cellular 916-804-2491 -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of John Bauer Sent: Monday, October 10, 2005 1:43 PM To: [log in to unmask] Subject: Re: [TN] Buss Bar Attachment Method Hi Franklin, 1. Does it need to be plated or can it be attached with nut-bolt? The current design which I have been asked to duplicate as close as possible has the buss bars as plated. There are a total of three bars. There are two on the input end and one on the output end of the board. On the input end there is one bar on top and one on the bottom and are offset from each other. These bars can have up to 450V between them. 2. Are there standoffs or other protrusions that can be inserted into the pcb? None. 3. Is this a solid bar or are there holes? Do the holes align with any holes on the board (i.e. tooling, contact, etc) The bars are solid with the exception to the two large treaded holes for aligning the bars in an assembly fixture and for attaching the lug from the end of a very heavy gauge wire when the assembly is complete. 4. Is this being attached at the beginning of the process, middle, end? Currently it is being attached in the beginning before anything else using a 250W hand-held soldering iron. 5. As for plating options, is there any reason it cannot remain bare copper? What is the environment it will be used in? heat, humidity, corrosive, neutral, sealed? The end application for this PCBA is to drive the motor of an electric car. This assembly does get warm. It is mounted on a large heatsink which is mounted in an enclosure with other PCBA's. Personally I would love to be able to attach these things with regular hardware but one of the engineers here says that this assembly is very sensitive and any added inductance can actually impact the way this assembly performs. I failed to mention in my earlier email that this PCB is fabricated with 10oz of copper. So not only do I have to deal with the bars being a big heatsink but the board is too. Best, ~John -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of John Bauer Sent: Monday, October 10, 2005 12:24 PM To: [log in to unmask] Subject: [TN] Buss Bar Attachment Method Greetings, We have an application where we will be attaching a buss bar that is 6 inches in length X .50 inch wide X .125 inch thick to the surface of our PCBA. The buss bar material is currently spec'd as full hard copper and is tin-lead plated. The .50 inch width side of the buss bar will be the surface soldered to the PCBA. My questions to you are 1) What process would be used to solder this bar to surface of the PCBA? 2) What plating options would be recommended other than tin-lead for this buss bar? The end use application for this will require that it handle 1000A of current in a worst case scenario. Thanks in advance, John Bauer --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------