Hi Susan, It is something you will have to adjust to.... Raise the reflow process temperature from 220 max to 230-235. This will allow the formation of reliable solder joints and hopefully not damage the rest of the parts. Handsolder the ones that are susceptible. I have used this process for almost two years with very little fallout but you should check the first board very closely to be sure that none of the connector bodies degrade. Phil Susan Mansilla <[log in to unmask]> wrote: Happy Friday to All I have a customer who is now being supplied with parts that the terminations are SnAgCu (95.5/4/0.5) instead of the previous SnPb. His process is not lead free and the parts are not always wetting and forming an adequate joint. What are his choices? Can he/should he take his SnPb line to lead free temps in an attempt to solder these parts - reflow process? Thanks for your advice Susan Mansilla Robisan Lab --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------