You mean you are taking a gold leaf out of the French book? :-) Brian Ofer Cohen wrote: > The wooden base under the coating. > > >>-----Original Message----- >>From: Judy Brown [mailto:[log in to unmask]] >>Sent: Thursday, October 27, 2005 22:21 >>To: TechNet E-Mail Forum; Ofer Cohen >>Subject: RE: [TN] (NTC) ENIG and brittleness >> >>And what was it that you saw in France? >> >>-----Original Message----- >>From: TechNet [mailto:[log in to unmask]] On Behalf Of Ofer Cohen >>Sent: Thursday, October 27, 2005 1:05 PM >>To: [log in to unmask] >>Subject: Re: [TN] (NTC) ENIG and brittleness >> >> After seeing today what I've seen in Versailes (France) I >>added for myself another reason for not using gold finish. >> >>Ofer Cohen >>Seabridge - a Siemens company >> >>--------------------------------------------------- >>Technet Mail List provided as a service by IPC using LISTSERV >>1.8e To unsubscribe, send a message to [log in to unmask] with >>following text in the BODY (NOT the subject field): SIGNOFF >>Technet To temporarily halt or (re-start) delivery of Technet >>send e-mail to >>[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE >>mailing per day of all the posts: send e-mail to >>[log in to unmask]: SET Technet Digest >>Search the archives of previous posts at: >>http://listserv.ipc.org/archives >>Please visit IPC web site >>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for >>additional information, or contact Keach Sasamori at >>[log in to unmask] or 847-615-7100 >>ext.2815 >>----------------------------------------------------- >> >> > > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 1.8e > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 > ----------------------------------------------------- > -- ______________________________________________ Please note new e-mail address [log in to unmask] --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------