Steve, I presume the fingers are nickel/gold plated. The gold can be replated using a plating wand but the nickel really cannot. It would be very difficult if not impossible to strip and replate all the edge connectors. Looks like the tape seal leaked during the plating process at the board vendor. At 09:37 AM 10/28/2005, you wrote: >Well, I just got back from "Sin City", and as they say; "no rest for the >wicked". > >I really wasn't that wicked, but I was confronted with a new problem this >morning. > >We just built some assemblies and conformal coated them, but when they were >being >de-masked, the gold plating on the fingers started peeling up! Check out: > >http://www.stevezeva.homestead.com/files/Peeling_Plating.jpg >http://www.stevezeva.homestead.com/files/Peeling_Plating_2.jpg > >I have a couple of questions: > >Can I repair this? > >If I repair this, should all fingers be stripped and repaired? > >Kind regards, > >-Steve Gregory- >Senior Process Engineer >LaBarge Incorporated >Tulsa, Oklahoma >(918) 459-2285 >(918) 459-2350 FAX >__________________________________________________________________ >This message may contain information that is privileged and confidential to >LaBarge, Inc. It is for use only by the individual or entity named above. >If you are not the intended recipient, you may not copy, use or deliver >this message to anyone. In such event, you should destroy the message and >kindly notify the sender by reply e-mail. > >--------------------------------------------------- >Technet Mail List provided as a service by IPC using LISTSERV 1.8e >To unsubscribe, send a message to [log in to unmask] with following text in >the BODY (NOT the subject field): SIGNOFF Technet >To temporarily halt or (re-start) delivery of Technet send e-mail to >[log in to unmask]: SET Technet NOMAIL or (MAIL) >To receive ONE mailing per day of all the posts: send e-mail to >[log in to unmask]: SET Technet Digest >Search the archives of previous posts at: http://listserv.ipc.org/archives >Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 >for additional information, or contact Keach Sasamori at [log in to unmask] or >847-615-7100 ext.2815 >----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------