Michael - for the 4553 specification, we tested IAg used with a soft touch membrane switch for 1000,000 cycles with no problems. The test was run over a prolonged period which allowed for the surface to tarnish but the results remained excellent. The data can be found in the appendix of the spec. We did not allow IAg to be used as a switch surface to be used for class 3 applications however. Regards Gerard O'Brien Photocircuits Corporation Co-chair 4-14 plating committee. -----Original Message----- From: Michael Forrester [mailto:[log in to unmask]] Sent: Monday, October 24, 2005 3:35 PM To: [log in to unmask] Subject: [TN] IAG used for keypad contacts Has anyone successfully used the IAG surface finish for keypad contacts instead of gold? Thank you. Best Regards, Michael Forrester Sr. Manufacturing Engineer LeCroy Corp. e-mail: [log in to unmask] --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------