Thank you all for your suggestions, Brian, the flux we are using is Alphametals 615-15 (ROL1) and I agree with you that the best action will be prevention. But now, to change all the connectors is not possible. So, we need to clean… We have tried to carry out the method proposed by George and although it works, we would like not add more rosin flux (the assembly is very complex) We know that IPA is not the best solution but it is a standard product. 141-b can damage other parts of the unit (by the way, I suppose that our company doesn’t purchase it in the black market) The new products suggested by Brian should be qualified before use in the process, and the “time flies”… Brian, can you recommend us other solution (easy to purchase, not toxic enough…)? I’m probably asking for a miracle. Thank you again Juan --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------