insufficient cure of the ink could do this Wolfgang ----- Original Message ----- From: "Franklin Asbell" <[log in to unmask]> To: <[log in to unmask]> Sent: Thursday, September 08, 2005 12:38 PM Subject: [TN] Pink symbol ink... > We got a call from a customer expressing an interesting issue. > > > > They ran product through their wave solder and the symbolization went from > white to pink. > > > > I've never heard of this color change appearing, anyone out there have an > idea? > > > > The symbol is Enthone 50-100R - white, the wave solder info I have is Type > R > flux with a peak temperature of 215 C. > > > > Appreciate any input, thanks. > > > > Franklin > > pI > > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 1.8e > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 > for additional information, or contact Keach Sasamori at [log in to unmask] or > 847-615-7100 ext.2815 > ----------------------------------------------------- > --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------