Looks to me like they did not reflow fully and therefore did not self-align as BGAs do. Jason Gregory Manufacturing Engineer Innova Electronics (281)653-5593 (281)653-5594 fax (281)212-0844 cell [log in to unmask] -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Bhandari, DS Sent: Friday, September 30, 2005 2:09 AM To: [log in to unmask] Subject: [TN] FW: bga image Dear All, Can anybody tell me whether these x-ray images are acceptable. I found that few outer ball are partially cut but still 90% pad is covered with the solder . I could not find any reference in workmanship standard for this kind of problem. Kindly help. <<83.tif>> <<076.tif>> Best Regards DS Bhandari - - - - - - - DISCLAIMER- - - - - - - - Unless indicated otherwise, the information contained in this message is privileged and confidential, and is intended only for the use of the addressee(s) named above and others who have been specifically authorized to receive it. If you are not the intended recipient, you are hereby notified that any dissemination, distribution or copying of this message and/or attachments is strictly prohibited. The company accepts no liability for any damage caused by any virus transmitted by this email. Furthermore, the company does not warrant a proper and complete transmission of this information, nor does it accept liability for any delays. If you have received this message in error, please contact the sender and delete the message. Thank you. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------