In a message dated 9/16/2005 9:10:09 AM Eastern Daylight Time, [log in to unmask] writes: Yep, they're buried vias and I think they're filled with resin. If they weren't filled they would look darker and the copper plating in the hole would look a lot rougher from the grinding & polishing. I think the hole fill was a separate operation (there's not enough pre-preg each side to fill the hole with resin). All the delam is on one side only, maybe there was some contamination of the layer during the filling. Geoff Layhe This seems to be Resin Coated Copper construction. The 1+4+1 construction is interesting - the four layer core is pretty standard (thick), but the added outer layer dielectric is quite thin. Definitely, there is not enough resin to fill the buried vias. It is hard to see from the magification here for sure that there is no glass in the surface dielectric. Check to be sure this is RCC construction. The treatment for RCC adhesion will be per the vendor's recommendation, and I suspect the board fab shop knows there were some shortcuts taken for them to give you the baking recommendations. If they also took shortcuts in pressing the parts to add the RCC layers, I doubt any procedure at this point will be sure to give you good boards after assembly. Denny Fritz MacDermid, Inc --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------