-----Original Message----- From: Clifford, Tom Sent: Thursday, September 29, 2005 12:14 PM Mike - Thanks for the view of all the TechNet thread on X-Ray damage. Very good discussions. Here's my summary and advice, which you might share with that forum: 1) "Voltage" settings /thresholds, etc alone mean NOTHING. Maybe worse than nothing, if somebody uses only voltage values to try to influence somebody. Total cumulative delivered dose is a function of voltage, certainly, but also amps (the dose is linear vs. power), and especially distance, optics, and certainly time, and off-angle position, and use of aluminum shields. All units differ, most shops' set-ups differ. Only if everything else is constant and known, only then can somebody say credible things like 10% higher voltage will deliver 10% greater dose rate; or double-the-current, double-the-dose; or 120 volts is the right operating limit, etc. Note that many X-Ray units have interacting operating parameters, so guidelines on dose rate vs. amps/volts, can get tricky. 2) The only way to convey credibility or to assure credibility is to define the situation properly. Steer way clear of folks who make wide sweeping reassurance statements. Be very wary of facile simplifications. 3) Ask your X-Ray supplier to look at your exact set-up, at your magnifications/ distances, at several operating levels; and give you actual received-dose data. Require that your sub-contract assemblers provide the same data. 4) Be especially mindful of exposure time. That's linear. Cooking a component under the beam while you futz with the image-enhancement or print-outs or referee decisions looking at the monitor, etc can all be silently detrimental. Set up a verification protocol and administrative controls, even using timers and buzzers, if necessary. 5) Do your own dosimetry. It's real easy. Dosimetry coupons are cheap and the tests take only minutes. You set the operating parameters and position the coupons to simulate your procedure, plus off-centerline positioning. You can get enough data to develop your shop protocols, to reassure your customers, and/or to guide/qualify your suppliers. 6)Components for sure differ in their vulnerability. I'm not confident that an assembler (like me) can generate that sort of vulnerability data. Get credible max-allowable-accumulative-dose values from device manufacturers, or from NASA or academia, not from X-Ray salesmen. New IC constructions, with finer geometries and odd new materials may be even more vulnerable. We use 100 Rad(sil) as a good conservative value ... that's a factor of 10 to 1000 conservative. but we are reappraising that threshold. 7) As mentioned in the messages below, the image you get at a given set of X-Ray conditions is influenced by lids and thermal-management add-ons and the board construction. The received-dose value is influenced also by board density and other-side parts' construction if the BGA is flip-side. All that needs to be modeled and built into your operating protocol. 8) Damage will not reveal itself real-time. You might think you have not damaged the part; hopefully, you haven't. Damage can show up later. Please do not tell your customers or yourselves that your process is OK because you observe no damage. Parts will not erupt in flames. Damage can be latent, sporadic, and subtle, and could easily escape simple continuity or functional tests. 9) Note also that many folks are also doing XRF measurements upstream to characterize lead finish (in the lead-free, tin-whisker hysteria). That dose can be significant, too; and is additive to what the part might see later in assembly in-process verification 10)IPC should step in to standardize the discussion, to provide procedures for characterizing your unit (settings and dosimetry tests) as well as to offer operating limits re accumulative dose. 11) IPC should also trigger and sponsor data and statements from the semiconductor/device/JEDEC folks, regarding standard, generic, and specific damage thresholds. my three cents worth Tom Clifford -----Original Message----- From: TechNet On Behalf Of Joyce Koo Jack, here is the reference regarding the issues. jk -----Original Message----- From: TechNet Behalf Of Jack Crawford Nick/Jack/Ken, if you look at the technet archives of the last several days you'll see a flock of msgs on this topic. Does JEDEC have any test methods or other guidance in place or proposed that would assist users with this issue? Because it is so closely focused on components I believe this would be more a JEDEC issue. Thanks Jack -----Original Message----- From: TechNet On Behalf Of Stadem, Richard I bet the folks at IPC are scrambling as well. ----Original Message----- From: TechNet On Behalf Of Franklin Asbell (chuckle) -----Original Message----- From: TechNet On Behalf Of Jason Gregory They probably all scrambled off to secret meetings as soon as Steve's Email surfaced. Jason Gregory -----Original Message----- From: TechNet Behalf Of Franklin Asbell Of course, and I'm thinking much of this would already have been performed, and data available, from the component suppliers. I never suggest taking on such a task without involving them, they're a valuable resource...and it's surprising none have spoken up yet. Franklin -----Original Message----- From: TechNet On Behalf Of Stadem, Richard The correct approach here is to establish a standard for how to test a particular component's susceptibility to X-ray exposure. The test methods would need to be established under one standard, the rating system under another standard. The rating system would need to include a method of measurement of exposure, both short term maximum exposure in Rems, and accumulative limits. -----Original Message----- From: TechNet On Behalf Of Jason Gregory Surely one could functionally test a known good part, then subject it to incrementally increasing amounts of X-rays to eventually arrive a failure point, then log the results...but could such a test be deemed accurate? I would imagine that different components (same part number, package, etc.) would suffer different levels of failure, however slight or large. Probably is true that the component makers just want to be sure, so they use substantially lower numbers to ensure that their products are "safe" and usable. But, at what point can the engineer, like Steve, say "130 kV is too much, but 90 kV is just fine". Just gambling. Jason Gregory ----Original Message----- From: TechNet On Behalf Of Michael Sewell Not to mention that the .050" core makes a good shield when x-rayed with the BGA on the top side, which is why we were turning the Kv up anyway. Now, if its on the bottom side during x-ray and nearly flush to the x-ray source..... ----Original Message----- From: TechNet Behalf Of Guy Ramsey This is one spooky thread. I know that NASA did some work on this subject, but I left my references back at ACI. There was nothing in it suggesting problems with X-ray inspection. They had some evidence that airport inspection equipment might damage sensitive components. -----Original Message----- From: TechNet Behalf Of Bev Christian And what about the possibility of resulting intermittent failures? Bev RIM -----Original Message----- From: TechNet Behalf Of Franklin Asbell My first question at such a technical meeting would be How much exposure will damage the part? I'm sure if you place the part in the chamber, turn on the x-ray and go to lunch you might have some problems. But would seconds, cause damage? What might be happening is component vendors want to protect their product and obviously so, so they place tighter than required standards on them, what is the time to failure under 90 kv at 20 mA, and at 50 mA, and at 90 mA? What is time to failure under 40 kv at 90 mA for 5 seconds? Or 30 seconds? Just some things I would try to answer during such an IPC technical activity. Franklin -----Original Message----- From: TechNet On Behalf Of Stadem, Richard Good Morning, Stephen! This is good information. So now we have component vendors telling us some of their components should not be overexposed to X-rays. Was there any type of notation on the part print? The industry needs a standard. We need to have some type of rating system for components that can be damaged by X-rays. Jack, is there any activity going on with this within IPC? -----Original Message----- From: TechNet Behalf Of Dehoyos, Ramon I would not be surprised if the X ray does damage some components depending on the intensity and the duration of the exposure. Part of the process in building a chip or IC is ion implantation. A material is doped positive or negative with respective ions, i.e. Ion implanter. Layer thickness is getting smaller every year, in the Angstroms, (1 micrometer = 10000 Angstroms = 0.001 millimeters = 0.0000394 inches ). The length of a transistor gate is 60 nanometers. I have also heard not to take some sensitive electronic equipment through X ray at the air ports due to the intensity of the exposure since several years ago from people that work with me and take electronic equipment all the time. Does anyone know someone that can do that type of experimentation or know someone that already have? Ramon -----Original Message----- From: TechNet On Behalf Of Charles Caswell Steve, I have heard of X-Ray erasing some memory but not actually damaging the component. -----Original Message----- From: Stephen R Gregory Hi Phil! The BGA in question is a small one, only 100-balls, and a plastic part with no heat-sink. It's on the bottom side of the board, and has to go through reflow one more time when the topside is built. As I said, everything looks fine at x-ray...it is inspected pretty closely too. Our customer is the one who is worried about x-ray, not us. They can't get the device to accept a program on some boards, and they are thinking that possibly x-ray damaged the device. Kind regards, ======================================== To: TechNet@IPC Stephen R Gregory/LABARGE) Hi Steve, I haven't ever heard of or experienced any issues with an x-ray inspection system causing damage to a chip. It is hard to believe that x-rays momentarily exposed to a chip could cause damage. I have seen some Altera BGAs that have difficulty getting good solder joint reflow due to the heat sinks on top of them, the PWBs 24 layers, and the sheer number of solderballs (1500+). With your .050" copper core, I would look at the thermal reflow and make sure that all the balls on the BGAs have fully collapsed. Was this BGA on the second side or first side reflowed? It is tough sometimes to tell where the problem is if you don't have a board level test in place. Phil -----Original Message----- From: TechNet Behalf Of Stadem, Richard I know of a few cases where over-exposure to X-rays has damaged certain components, most often CMOS components. Some CMOS EEPROM components can even be damaged by overexposure to UV light. It is not very likely, but it is definitely quite possible. It has happened, and it is a concern. If you are looking at a particular area on a PWA, the adjacent areas are also being exposed. If you continue to go back and look at that area, the total accumulated dose can hurt certain CMOS components (and other types as well). It is not very likely, but there are steps you can take to prevent inadvertent damage from overexposure. Again, read Tom Clifford's article on the subject. -----Original Message----- From: TechNet On Behalf Of Steve Gregory I submitted a question to Altera via their email support center about x-ray inspection possibly damaging a EPM7256EEFI100-7 device. The device is a EEPROM made using an advanced CMOS process. Here is our exchange so far: Request No: 10515187 Status: Close-Pending Date Opened (PDT): 9/26/2005 >Description: I am doing x-ray inspection of a EPM7256AEFI100-7 device after board assembly. >The PCB has a 1.27 mm thick copper core in the center of it, so it >requires that a high kv x-ray must >be done in order to see the solder connections of the device. The x-ray source power is around >120-130 kv. Will this x-ray power level damage the device?, =================== >To Customer: >Hi Stephen, Typically assembly uses 90 KV using 10 to 20 mA with a few second for inspection of IC package. Our recommendation will be a pro-rated 130 KV with 7 mA to 13 mA for a few second. Note that Prolong exposure under X-ray will definitely damage the device. I hope it's helpful to you. Best Regards, Daniel Cao My question is; doesn't the figure of 90 KV at 10-20 mA seem pretty low? My current Glenbrook RTX-113 operates at 35-52 KV at 20-50 mA, and higher-end Glenbrook systems will pump 70-90 KV at 90-100 mA. Right now, I'm using a Fein Focus Tiger 160 for x-ray inspection of some copper cored assemblies that we're building because I have to, that's the only way we can inspect the BGAs. The copper core in the PCB won't allow x-ray of the BGAs unless you use a system that can penetrate the core. But if these devices can be damaged at such a low voltage (if indeed Daniel's figures are correct), shouldn't Altera issue some sort of warning to their customers about x-ray damaging the devices? After all, there will be a lot of customers using x-ray for inspection. -Steve Gregory- -----Original Message----- From: TechNet Behalf Of Guy Ramsey A couple of years ago, NASA published a warning. They required anyone transporting via air to hand carry them onboard. The warning had to do with high energy X-ray used at some facilities to luggage inspection. They did not, as I recall, establish any acceptable level of exposure. I haven't heard anything lately. But, you might bounce this one off the EMPF Helpline. -----Original Message----- From: TechNet Behalf Of Joyce Koo http://www.sandia.gov/media/rhp.htm -----Original Message----- From: TechNet Behalf Of Stadem, Richard I have had to address the same concerns for Aerospace programs. I have not been able to find any formal standards for radiation exposure limits. All I found was a good paper on the subject from Tom Clifford at Lockheed Martin ("X-Ray Inspection, Easy Does It" in EP+P magazine) I also talked to two X-ray vendors and they tell me that even if the typical X-rays were cranked up to 120 kv or about 3-5 watts, a component would have to be exposed for a full day or longer to accumulate enough total Rems such that it could hurt the component, and that the only types of components that could be possibly damaged would be CMOS memory. I have found some information on protecting components in space systems from natural X-rays, but nothing on process-generated X-rays. Everybody tells me it is not a problem. This is not enough for me, so I asked the folks at IPC but have not heard a response as yet. Anyone else know of any standards for limitations of X-ray emissions on electronic components? --Original Message----- From: TechNet Behalf Of Steve Gregory Sent: Monday, September 26, 2005 11:17 AM To: [log in to unmask] Subject: [TN] X-ray inspection, can it damage devices? Good Mornin' Everyone! I hope you all had a good weekend! I worked Saturday, but had Sunday off. Sat around Sunday and watched the NASCAR race at the "Monster Mile" in Dover Delaware. 20-year old Kyle Busch gave Jimmie Johnson a run for his money finishing second at the green/white/checkered ending....but I digress..... Anyways, we built an assembly here that has a .050" copper core in the center of it...not the same assembly as the one I did my "okie cross-section" on). It is double-sided SMT, and has BGAs on both sides. I'm doing x-ray inspection with a Fein Focus Tiger 160, and in order to penetrate the core and do a proper inspection of the solder joints and spheres of the BGAs, the x-ray power is up around 120-130 kv. Our customer received a number of the assemblies from us (without test from us, as they are prototypes and test hasn't been developed yet), and they are having problems with one of the BGAs. It's a 100-ball Max-7000 device from Altera, a CMOS EEPROM, and our customer has been trying to program the device via on-board programming, but some boards wont program. The x-ray inspection turned out fine. All BGAs were inspected using oblique angles, so if there was an open joint, it would have been seen. They are worried that maybe the x-rays may have damaged the device. Altera has told our customer that the x-rays shouldn't hurt the device. I've got a case number started via email in to Altera (since I can't talk to anyone on the phone), asking them myself if x-rays will damage the device. I'm also going to call Fein Focus and talk to them as well. But have any of you ever heard of x-ray damaging BGAs? Kind regards, --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------