I have not heard of doing this. I have heard of vapor honing for adhesion promotion for electroless copper. At 07:34 AM 09/06/2005, you wrote: >Dear Technetters, > >I'm not familiar with the process of making pcb and I would like to >have your comments on something I was told from a pcb maker >representative. > >"...in order to ensure a well insulation between traces, we do >sandblasting (very little and tiny) pcb's after etching. >this is to remove the bonding material that remains on the board after >removing the copper. This is the only way to achieve a very good SIR >result." > >Is this a normal procedure, was he correct in his claim? > > >Thanks, >Ivanoe Pedruzzi > >--------------------------------------------------- >Technet Mail List provided as a service by IPC using LISTSERV 1.8e >To unsubscribe, send a message to [log in to unmask] with following text in >the BODY (NOT the subject field): SIGNOFF Technet >To temporarily halt or (re-start) delivery of Technet send e-mail to >[log in to unmask]: SET Technet NOMAIL or (MAIL) >To receive ONE mailing per day of all the posts: send e-mail to >[log in to unmask]: SET Technet Digest >Search the archives of previous posts at: http://listserv.ipc.org/archives >Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 >for additional information, or contact Keach Sasamori at [log in to unmask] or >847-615-7100 ext.2815 >----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------