Bob: In general I would recommend two part epoxy designed for metal bonding. Loctite/Hysol's E-20NS is an example. There are many others available. However you do not provide much detail as to the required cured properties and environmental exposure. More information could dictate a different adhesive type. Regards Michael Barmuta Staff Engineer Fluke Corp. Everett WA 425-446-6076 -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Bob Arciolla Sent: Friday, September 23, 2005 11:09 AM To: [log in to unmask] Subject: [TN] bonding material Hi all, I have a unit that we manufacture that has a aluminum case and cover and was wondering if anyone can recommend a bonding material for this and where to get it. Thanks in advance, Bob Arciolla Endicott Research Group --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- Quality/Safety Manager --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------