And the co-worker was cleared of any blame in the accident but immediately arrested because analysis of the nails showed unacceptably high traces of hexavalent chromium......................8-) John ------------------------------------ Avanex John Burke Senior Manager RoHS Compliance [log in to unmask] 40919 Encyclopedia Circle Fremont CA 94538 tel: 510 897 4250 fax: 510 979 0189 mobile: 510 676 6312 ------------------------------------ -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Steve Gregory Sent: Friday, September 16, 2005 9:58 AM To: [log in to unmask] Subject: [TN] OT Bad Day at Work... It's been a while since I've posted a OT "Friday", type of email. Seeing how it's at the end of the week, it's at a time we all reflect back on the past weeks toils and struggles. A time where some of us have been able to accomplish the things that we intended to accomplish, and a time where some of us had really bad days at work. When you say you've had a bad day at work, just how bad was it? I've got an example of someone who has had a really, really bad day at work. Check this out: http://www.stevezeva.homestead.com/files/Bad_Day.doc I've had bad days at work, but nothing like this guy did. In fact, all my bad days at work have been good days in comparison to his... -Steve Gregory- __________________________________________________________________ This message may contain information that is privileged and confidential to LaBarge, Inc. It is for use only by the individual or entity named above. If you are not the intended recipient, you may not copy, use or deliver this message to anyone. In such event, you should destroy the message and kindly notify the sender by reply e-mail. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------