Rudy and others, The copper mirror test is a simple look-and-see test that can be used as part of the qualification of a flux, solder paste, or any other chemical that may come in contact with a printed circuit board or printed circuit pack. See IPC-TM-650, Test Method 2.3.32D. Essentially a flux or material is dissolved in IPA (or at least sort of), applied to a vapour deposited copper mirror, the solvent is allowed to evaporate and then the mirror is stored at RT and 50%RH for 24 hours and then you wash off the material and see whether it has eaten through the thin copper mirror coating. Now if you are using water as the solvent, the vapour pressure is much lower. I can't remember what I used to do when I did this test at Nortel in the late 90's when we started to use the water-based wave solder fluxes. Bev RIM _____ From: R Sedlak [mailto:[log in to unmask]] Sent: August 17, 2005 3:41 PM To: TechNet E-Mail Forum; Bev Christian Subject: Re: [TN] Copper Mirror test for water-based fluxes For those of us who only recently realized that something had to happen to a PCB before it was installed..(Assembly? What's that?)... be so kind as to tell us more about this test, and what it is supposed to tell you... and how to read it.... Any help is appreciated...(and needed) Rudy Sedlak RD Chemical Company Bev Christian <[log in to unmask]> wrote: It is such a long time that I have done one of these, that I don't remember what we did to evaporate the water! The alcohol based ones are easy, but the water ones?! Do you just let them set at room temperature or do you give them a little heat or what? Bev RIM --------------------------------------------------------------------- This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- __________________________________________________ Do You Yahoo!? Tired of spam? Yahoo! Mail has the best spam protection around http://mail.yahoo.com --------------------------------------------------------------------- This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------